The highest degree of cleanliness, the lowest degree of segregation of alloy elements and decreased sulphur content along with a homogenous structure and excellent characteristics with their ESR process, Saarschmiede sets quality measures, even for very heavy forging ingots of up to 165 t.
The ingots are characterized by their optimum degree of sulphuric and oxidic cleanliness as well as
an even solidification structure throughout the whole length and cross-section of the ingot |
 |
|
|
Electro Slag Remelting Facility (ESR) |
|
 |
|
2 Melting Stations
· Ingot weights up to 165 t
· Ingot weights up to 8 t |
|
|
|